Seamless heat-resistant steel tube DIN17175

Din17175 Boiler Tube description

DIN 17175 is a specific standard developed by the German Institute for Standardization (DIN) for seamless steel tubes for boilers and pressure vessels, focusing on material reliability under high temperature and high pressure conditions. Its core mission is to ensure the safe operation of pipelines in thermal systems (such as power plant boilers and chemical reactors), with particular emphasis on high-temperature creep resistance and long-term structural stability.

 

Chemical Compositions of DIN 17175

Grade C Si Mn P S Cr Mo
St35.8 ≤0.17 0.10-0.35 0.40-0.80 ≤0.040 ≤0.040 / /
St45.8 ≤0.21 0.10-0.35 0.40-1.20 ≤0.040 ≤0.040 / /
15Mo3 0.12-0.20 0.10-0.35 0.40-0.80 ≤0.035 ≤0.035 / 0.25-0.35
13CrMo44 0.10-0.18 0.10-0.35 0.40-0.70 ≤0.035 ≤0.035 0.70-1.10 0.46-0.65
10CrMo910 0.08-0.15 ≤0.50 0.40-0.70 ≤0.035 ≤0.035 0.20-0.25 0.90-1.20

 

Mechanical Properties of DIN17175

Grade Yield Strength (Mpa) Tensile Strength (Mpa) Elongation(%)
St35.8 ≥235 360-480 25
St45.8 ≥255 410-530 21
15Mo3 ≥275 450-600 20
13CrMo44 ≥290 440-590 20
10CrMo910 ≥280 450-600 18

 

DIN17175 V.S A179

Dimension DIN 17175‌ (German Standard) ASTM A179‌ (U.S. Standard)
Core Purpose High-pressure boiler piping‌ (steam temp ≥450°C) Condenser tubes for heat exchangers‌ (low-temp applications)
Material Type Heat-resistant steel (carbon/Cr-Mo alloy) Low-carbon steel (non-alloy)
Service Temp Up to 650°C‌ (Grade 10CrMo910) ≤450°C‌ (overheating causes oxidation failure)
Tensile Strength 450-600 MPa (e.g., 15Mo3) ≥325 MPa
Yield Strength @500°C ≥180 MPa‌ (mandatory) Not tested (non-high-temp tube)
Carbon Content ≤0.20% 0.06-0.18%
Key Inspection Decarb depth ≤0.3mm + 520°C tensile test Eddy current test + hydrostatic test

 