What Is S275JR RHS Tube?
S275JR rectangular hollow section (RHS) tube is a structural steel product whose base material is defined in EN 10025-2. The grade name is decoded as follows: S means structural steel, 275 means the minimum yield strength is 275 MPa, and JR means the steel must achieve a minimum Charpy impact energy of 27 J when tested at 20 deg C. RHS is the rectangular form of hollow section, with two unequal side dimensions, and it is manufactured as hot-finished sections to EN 10210-1 or as cold-formed welded sections to EN 10219-1.
Because the rectangular profile can be oriented with its strong axis in the direction of the main load, RHS is often more material-efficient than a square section when bending is dominant in one plane. It is a workhorse grade in European structural steelwork and is exported worldwide under EN specifications.
Chemical Composition
The chemical limits below apply to S275JR with product thickness up to 40 mm:
| Element | Requirement, % |
|---|---|
| Carbon (C), max | 0.21 |
| Manganese (Mn), max | 1.50 |
| Phosphorus (P), max | 0.035 |
| Sulfur (S), max | 0.035 |
| Nitrogen (N), max | 0.012 |
| Copper (Cu), max | 0.55 |
The low carbon content keeps the steel readily weldable and cold-workable. Manganese provides the main strengthening contribution, while phosphorus, sulfur and nitrogen are tightly limited to preserve toughness and weld quality. Some specifications allow a small copper addition to improve resistance to atmospheric corrosion.
Strength and Mechanical Properties
The mechanical values of S275JR change slightly with product thickness:
| Property | Thickness <= 16 mm | Thickness 16 - 40 mm | Thickness 40 - 63 mm |
|---|---|---|---|
| Minimum yield strength | 275 MPa | 265 MPa | 255 MPa |
| Tensile strength | 410 - 560 MPa | 410 - 560 MPa | 410 - 560 MPa |
| Minimum elongation | 22 % | 21 % | 19 % |
| Minimum impact energy at 20 deg C | 27 J | 27 J | 27 J |
Yield strength defines the onset of permanent deformation and is the value normally used for allowable-stress design. Tensile strength defines the ultimate load capacity and the material resistance to fracture. Elongation measures the plastic deformation available before rupture, and impact energy measures resistance to brittle fracture under dynamic loading at room temperature.
Delivery Conditions and Processing
S275JR RHS tube is typically supplied in one of the following base-material delivery conditions:
Hot rolled: the strip or section is cooled directly after high-temperature rolling. This is the economical default and satisfies most structural applications. Controlled rolling: rolling temperature and reduction are controlled to refine the grain structure, improving both strength and toughness. Normalizing: the product is heated to the appropriate temperature and air-cooled to homogenize the structure and refine grain; a normalized product is designated S275JR+N and is preferred for demanding or thick-section applications.
Further processing is available to suit the project: cutting to length by sawing, laser, plasma or flame; non-destructive testing (for example ultrasonic, eddy current or magnetic particle inspection) at the required level; and through-thickness (Z-direction) property testing, with Z15, Z25 or Z35 classes, for joints loaded in the thickness direction where lamellar tearing is a risk.
Applications
Building structures: columns, beams and bracing for high-rise buildings and industrial plants, where the hollow section reduces weight while providing sufficient load capacity and seismic performance. Bridge engineering: support structures and cross-bracing where weldability and predictable toughness are essential. Shipbuilding: deck beams, hull stiffeners and superstructure members that benefit from corrosion protection systems and good weldability. Machinery manufacturing: equipment frames, bearings housings and transmission supports under complex loads. Non-pressurized storage and process supports: tank skirts, pipe racks and access platforms. Note that S275JR is a structural grade and should not be used for the pressure boundary of pressure vessels; pressure-vessel grades such as P265GH are the correct choice for that duty.
Selection Considerations
Confirm the design thickness before ordering, because yield strength steps down from 275 MPa at 16 mm to 265 MPa at 40 mm and 255 MPa at 63 mm. If the structure will be exposed below 20 deg C, select a grade with a lower impact-test temperature such as S275J0 or S275J2. For welded nodes with heavy restraint or thick walls, specify a normalizing delivery condition and a suitable preheat. Always request the mill certificate (EN 10204 3.1) and verify that the delivered chemistry and mechanical results match the ordered grade, especially when the tube is intended for certified structures.
Frequently Asked Questions
What is the yield strength of S275JR RHS tube?
The minimum yield strength is 275 MPa for wall thickness up to 16 mm, 265 MPa for 16 - 40 mm, and 255 MPa for 40 - 63 mm. The nominal grade value used in trade is 275 MPa.
What is the tensile strength of S275JR?
Per EN 10025-2 the tensile strength is 410 - 560 MPa for all common thicknesses up to 63 mm. The lower end of the range governs design for connections and ultimate loads.
Is S275JR suitable for pressure vessels?
No. S275JR is a structural steel, not a pressure-vessel steel. For pressure-retaining parts of boilers and vessels, use pressure grades such as P265GH (EN 10028-2) or the equivalent national grade, which have specified high-temperature properties and tighter quality requirements.
What does the +N delivery condition mean?
The +N suffix means the steel is delivered in the normalized condition, which refines the grain structure and improves toughness and uniformity. Normalized material is designated S275JR+N and is often required for thick plates and sections or for cold-climate structures.
Can S275JR RHS be cold-formed into curved sections?
Yes, but the bending radius should be large enough to avoid cracking at the corners of the section. As a rule of thumb, the inside bend radius should be several times the section depth, and the operation should be checked against the elongation capacity of the grade. Hot bending is an alternative for tight radii.
How is RHS different from SHS?
RHS is rectangular (two different side dimensions) while SHS is square (equal sides). Both are hollow sections governed by the same EN 10210-1 and EN 10219-1 standards. RHS gives higher bending stiffness in one direction when oriented accordingly, which is why it is favored for beams and girders.