UNS S32750 Seamless Steel Pipe

Feb 19, 2024 Leave a message

2507 stainless steel pipe, UNS S32750 seamless steel pipe
2507, UNS S32750, products include: bars, bars and profiles, plates, sheets and strips, seamless and welded nominal pipes, coal-jointed nominal pipes, seamless and welded pipe fittings, pipe fittings, forged or rolled pipes Flanges and forged pipe fittings, forged waste materials and rods.
Chemical composition %: Nickel (Ni): smaller than 6.0, larger than 8.0, Iron (Fe): balance, (Cr): smaller than 24.0, larger than 26.0, (M) smaller: 3.0, larger than 5.0, Carbon (C): greater than 0.030, manganese (Mn): greater than 1.20, silicon (Si): greater than 0.80, phosphorus (P) greater than 0.035, (S): greater than 0.020, copper (Cu) greater than 0.5, ( N): Small: 0.24, Larger: 0.32.
Production standards include: ASTM A276, A484 for regular materials, bars and profiles, ASTM A240, A480 for medium plates, sheets and strips, ASTM A790, A 999 for seamless and jointed pipes, ASTM A789, A1016 For seamless and welded pipe fittings, ASTM A815, A960 for pipe fittings, ASTM A182, A961 for forged or rolled pipe flanges and forged pipe fittings, ASTM A314, A484 for forging scrap and rods
Physical properties: 7.75 g/cm3, melting point: 1396-1450°C.
characteristic:
2507 is a super duplex stainless steel with better corrosion resistance and strength than 2205. It combines the more beneficial properties of many ferritic steels and austenitic steels. Since the steel has high chromium and molybdenum content, it has very good resistance to uniform corrosion, pitting corrosion and crevice corrosion. The dual-phase preparation ensures that the steel has high resistance to stress corrosion cracking and also has high mechanical strength.
The higher chromium and molybdenum content makes it have strong resistance to overall corrosion against agricultural production system acids such as acid, acetic acid, etc. It also has strong resistance to corrosion against inorganic acids, especially those containing chlorides. ability. Compared with 904L, which is specially designed to resist the corrosion of pure sulfuric acid, 2507 has stronger corrosion resistance against dilute sulfuric acid mixed with chloride ions. Grade 316L cannot be used in hydrochloric acid environments, as it may suffer local corrosion or overall corrosion, while 2507 can be used in dilute hydrochloric acid environments and has strong resistance to spot damage and crack corrosion. The lower carbon content of 2507 greatly reduces the risk of intermediate carbide precipitation during heat treatment. Therefore, it has strong resistance to carbide-related intergranular corrosion. 2507 has high compressive strength, impact strength, low thermal expansion coefficient and high thermal conductivity. These characteristics are suitable for many structural parts and mechanical components. 2507 should not be exposed to temperatures above 300°C for a long time, as this may weaken its toughness.
application:
Chemical industry pipelines, containers, heat exchange liquids, seawater pipelines in desalination plants, oil and gas industry equipment, power plant flue gas desulfurization systems, washing equipment, absorption towers, chemical liquid tank trucks.

Stainless Steel Hollow Pipe