EN 10216 Seamless Steel Tubes for Pressure Purposes

Oct 20, 2025 Leave a message

What the EN 10216 Series Contains

EN 10216 is the European standard for seamless steel tubes for pressure purposes. It is divided into five parts, each aimed at a different material family or a different service temperature band, and together they cover the seamless tube needs of boiler, pressure vessel and piping construction.

EN 10216-1: seamless tubes of non-alloy steel with specified room temperature properties.

EN 10216-2: seamless tubes of non-alloy and alloy steel with specified elevated temperature properties.

EN 10216-3: seamless tubes of alloy fine grain steel with specified low temperature properties.

EN 10216-4: seamless tubes of non-austenitic stainless steel.

EN 10216-5: seamless tubes of austenitic stainless steel.

Every part follows the same internal logic. It lists the steel grades it covers, the upper and lower limits of their chemical composition, the mechanical property values at room temperature and, where relevant, at elevated temperature, the heat treatment condition at delivery, and the inspection and testing requirements. That structure means a buyer can place a single order reference and obtain a fully traceable material definition.

Grades Covered by EN 10216-1

The room temperature part of the series uses six non-alloy grades. The TR1 variants are supplied with a normal impact testing regime, while the TR2 variants carry an additional low temperature impact requirement of at least 40 J average, which makes them suitable for colder climates and for thicker sections where brittle fracture resistance matters. The steel numbers below are used together with the grade names on mill certificates and on fabrication drawings.

Grade Steel number Impact requirement
P195TR1 1.0107 Standard
P195TR2 1.0108 ≥ 40 J average
P235TR1 1.0254 Standard
P235TR2 1.0255 ≥ 40 J average
P265TR1 1.0258 Standard
P265TR2 1.0259 ≥ 40 J average

Chemical Composition

All six grades are low carbon, fully killed steels with tightly controlled residuals. Manganese increases with grade to provide the extra strength, and the sum of chromium, copper, molybdenum and nickel is capped at 0.70% to keep the steel clean and weldable.

Steel grade C max, % Mn max, % P max, % S max, % Cr max, % Mo max, % Ni max, % Cu max, % Nb max, % Cr+Cu+Mo+Ni max, %
P195TR1 0.13 0.70 0.025 0.020 0.30 0.08 0.30 0.30 0.010 0.70
P195TR2 0.13 0.70 0.025 0.020 0.30 0.08 0.30 0.30 0.010 0.70
P235TR1 0.16 1.20 0.025 0.020 0.30 0.08 0.30 0.30 0.010 0.70
P235TR2 0.16 1.20 0.025 0.020 0.30 0.08 0.30 0.30 0.010 0.70
P265TR1 0.20 1.40 0.025 0.020 0.30 0.08 0.30 0.30 0.010 0.70
P265TR2 0.20 1.40 0.025 0.020 0.30 0.08 0.30 0.30 0.010 0.70

Aluminium is added for deoxidation and grain refinement, and a minimum total aluminium content applies to each grade. Niobium is restricted to a maximum of 0.010% so that the steel remains predictable during hot forming and welding.

Mechanical Properties

Tensile and yield values are specified at room temperature, and the yield figure refers to the upper yield strength ReH for these ferritic grades. The TR2 variants are additionally impact tested, with a minimum average absorbed energy of 40 J.

Standard Steel grade Tensile strength, MPa Yield strength min, MPa Elongation min, % Impact energy, J
EN 10216-1 P195TR1 320-440 195 27 -
EN 10216-1 P195TR2 320-440 195 27 ≥ 40
EN 10216-1 P235TR1 360-500 235 25 -
EN 10216-1 P235TR2 360-500 235 25 ≥ 40
EN 10216-1 P265TR1 410-570 265 21 -
EN 10216-1 P265TR2 410-570 265 21 ≥ 40

Ordering Details: Ends, Packing and Inspection

Tubes are supplied with square cut plain ends, beveled ends for welding or threaded ends where a screwed connection is required. Surface condition is either as rolled, pickled or machined, depending on the size and the agreed delivery condition. Packing is normally in bundles or in wooden cases, and seaworthy packing can be arranged when the tubes travel by sea.

Hydrostatic testing is applied to each tube as a pressure integrity check, with the test pressure calculated from the tube dimensions and grade.

Eddy current testing is the standard non-destructive examination for the series; ultrasonic testing can be added for longitudinal defect detection.

Flattening, flaring and bending tests demonstrate the ductility of the tube and the soundness of the tube ends.

Marking covers the standard, the grade, the heat number, the size and the test status, so that the tube can be traced back to its mill certificate.

FAQ

Q: Which part of EN 10216 applies to room temperature service?
EN 10216-1 covers non-alloy seamless tubes with specified room temperature properties and is the usual choice for general pressure piping and structural pressure parts.

Q: What is the difference between TR1 and TR2 grades?
TR1 grades meet the base tensile and elongation requirements, while TR2 grades carry an additional impact test with a minimum average absorbed energy of 40 J.

Q: Are EN 10216 tubes seamless?
Yes. The whole EN 10216 series describes seamless tubes; welded pressure tubes are standardised separately in the EN 10217 series.

Q: What does the steel number such as 1.0254 indicate?
It is the European material number for the grade. P235TR1 is 1.0254, and the number is quoted alongside the grade name on inspection documents.

Q: How is the delivered length controlled?
Lengths are supplied as random, approximate or exact. When exact lengths are ordered, the tolerances of the dimensional standard apply, and cut lengths are marked before packing.

Q: Can EN 10216-1 tubes be used at elevated temperature?
Not for creep range service. Once the design temperature exceeds the room temperature band, a grade from EN 10216-2 should be selected instead.