AISI 1035 Steel: Properties, Heat Treatment, and Applications

Nov 19, 2025 Leave a message

What Is AISI 1035 Steel?

AISI/SAE 1035 is a medium-carbon plain carbon steel grade. With a nominal carbon content of about 0.32-0.38%, it is stronger than low-carbon steels such as 1018 but more ductile and easier to form than higher-carbon grades such as 1045 or 1060. The grade number follows the SAE/AISI system, where the first two digits indicate the steel family (10 = plain carbon, non-resulfurized) and the last two digits give the nominal carbon content in hundredths of a percent.

Chemical Composition

Element Content (%)
Carbon (C) 0.32 - 0.38
Manganese (Mn) 0.60 - 0.90
Phosphorus (P) 0.040 max
Sulfur (S) 0.050 max

The chemistry is verified by heat (cast) analysis and, when required, by product analysis with the permitted deviations of the relevant specification.

Mechanical Properties

Typical hot-rolled values for 1035 steel are: tensile strength about 570-620 MPa, yield strength about 310-370 MPa, and elongation about 18-25% in 50 mm. Actual values depend on section size, condition and heat treatment. The moderate carbon content gives a practical balance of strength and ductility, although the material can work-harden during machining, which may increase tool wear and affect chip formation.

Heat Treatment

Annealing is typically performed at about 800 °C (1475 °F) with sufficient holding time, followed by slow furnace cooling to relieve internal stresses and soften the steel for machining. Normalizing refines the grain after hot working, and hardening by quenching followed by tempering develops higher strength and hardness for engineering components.

1035 vs 1045

Property 1035 1045
Carbon content 0.32 - 0.38% 0.43 - 0.50%
Strength Moderate Higher
Ductility and formability Better, easier to work Lower
Machinability Good Good, slightly harder
Typical use Shafts, studs, general parts Axles, gears, higher-strength parts

Choose 1035 when formability and machining ease matter; choose 1045 when higher strength and wear resistance are the priority.

Weldability

1035 steel is generally weldable with common processes such as MIG, TIG and stick welding. Because the carbon content is medium, preheating and controlled cooling are recommended for thicker sections to avoid hardening and cracking in the heat-affected zone. Post-weld heat treatment may be required for highly restrained joints.

Applications

Typical applications include shafts, studs, bolts, gears, machine parts, forged components and general engineering parts requiring higher strength than low-carbon steels. It is also used for pipe and tube products in mechanical and structural applications.

FAQ About 1035 Steel

Is 1035 a low-carbon steel?

No. With 0.32-0.38% carbon it is classified as a medium-carbon steel.

Is 1035 the same as ASTM A36?

No. A36 is a structural steel with lower strength and no tight composition control; 1035 is a medium-carbon engineering steel with defined chemistry and higher strength.

What is the annealing temperature for 1035?

Annealing is typically carried out at about 800 °C (1475 °F), holding for sufficient time, then cooling slowly in the furnace.

Can 1035 be hardened by quenching?

Yes. It responds to quench and temper heat treatment, though its hardenability is moderate because it is a plain carbon steel; oil or water quenching is used depending on section size.

Why does 1035 work-harden during machining?

The moderate carbon content increases the flow stress of the chips, causing strain hardening at the cutting zone; using sharp tools, adequate coolant and appropriate speeds reduces tool wear.

What is the difference between 1035 and 1045?

1045 has higher carbon (0.43-0.50%) and therefore higher strength and hardness but lower ductility. 1035 is easier to form and machine.