What Is S275JR SHS Tube?
S275JR square hollow section (SHS) tube is a structural steel product made from S275JR grade material defined in the European standard EN 10025-2. The grade name is a code: S indicates structural steel, 275 is the minimum yield strength in megapascals, and JR specifies a minimum impact energy of 27 J at 20 deg C. SHS tube is produced in square cross-sections with a hollow interior, giving a very high strength-to-weight ratio compared with solid sections or open profiles.
The material is classed as a non-alloy (mild-to-medium carbon) structural steel with controlled impurity limits, and it is widely used in buildings, bridges, machinery frames, shipbuilding and energy equipment because it combines economy with balanced strength, weldability and toughness. Its density is approximately 7.85 g/cm3, the same as other structural carbon steels.
Chemical Composition
The composition of S275JR is balanced to give adequate strength without sacrificing weldability. The limits below apply to product thickness up to 40 mm per EN 10025-2:
| Element | Requirement, % | Role |
|---|---|---|
| Carbon (C), max | 0.21 | Controls hardenability and weldability |
| Manganese (Mn), max | 1.50 | Solid-solution strengthening, improves toughness |
| Silicon (Si), max | 0.55 | Deoxidation, fine strength adjustment |
| Phosphorus (P), max | 0.035 | Impurity, kept low to avoid brittleness |
| Sulfur (S), max | 0.035 | Impurity, kept low for weld quality |
| Nitrogen (N), max | 0.012 | Impurity, controlled for toughness |
| Copper (Cu), max | 0.55 | Improves atmospheric corrosion resistance |
These limits ensure the steel can be cut, cold-formed, drilled and welded by conventional methods without special precautions in most sections.
Tensile and Mechanical Properties
The key mechanical values of S275JR are defined by thickness in EN 10025-2:
| Property | Thickness <= 16 mm | Thickness 16 - 40 mm |
|---|---|---|
| Minimum yield strength | 275 MPa | 265 MPa |
| Tensile strength | 410 - 560 MPa | 410 - 560 MPa |
| Minimum elongation (longitudinal) | 22 % | 21 % |
| Impact energy at 20 deg C, min | 27 J | 27 J |
When SHS tube is produced to EN 10210-1 (hot-finished hollow sections) or EN 10219-1 (cold-formed welded hollow sections), the mechanical values of the finished tube must still meet the EN 10025-2 requirements for the base material. In practice, yield strength and tensile strength are the values that dominate section design, while elongation and impact energy protect against brittle failure in service and during erection.
SHS Tube Size Range and Manufacturing
SHS tube is commonly available in side lengths from about 20 mm up to 400 mm, with wall thicknesses from 1.5 mm to 16 mm. The manufacturing route starts with hot-rolled strip, which is slit to width, cold-formed into a square profile, and closed by high-frequency electric-resistance welding. The weld is then annealed or normalized locally, the tube is sized and straightened, and internal and external weld beads are trimmed. Tolerances on side length, wall thickness, straightness and corner profile follow EN 10219-1 or the project specification.
Applications
S275JR SHS tube is used wherever a square hollow section gives the most efficient load path for the material weight:
Building structures: factory steel beams, stair stringers, columns, roof trusses and connectors. Heavy machinery: crane booms, excavator chassis members and conveyor trusses. Transportation equipment: trailer chassis, container corner posts and ship internal structures. Infrastructure: bridge secondary members, power transmission tower bracing and sign gantries. Because the square section offers equal bending resistance in the two principal axes and flat faces that simplify bolted and welded joints, it is a default choice for space frames and modular construction.
Selection and Fabrication Points
Choose the grade S275JR only when the design yield of 275 MPa is sufficient and the service temperature is not below the impact-test temperature; for cold climates, a sub-zero impact grade such as S275J2 is required. For welding, the low carbon equivalent keeps crack sensitivity low, but in thick-walled sections preheat and controlled interpass temperature are still good practice. When bending SHS, the bend radius should respect the wall-thickness-to-side-length ratio to avoid corner cracking, and hot bending should be followed by a check of the affected zone. Order material with a mill certificate confirming the heat number and the EN 10204 3.1 inspection document if the project requires traceability.
Frequently Asked Questions
What is the tensile strength of S275JR SHS tube?
Per EN 10025-2, the tensile strength of S275JR is 410 - 560 MPa across common thicknesses. The minimum yield strength is 275 MPa for thickness up to 16 mm and 265 MPa for 16 - 40 mm. These are the values to use in structural design.
Is S275JR the same as Q275 steel?
Not exactly. S275JR is the European EN designation; Q275 is the corresponding Chinese standard grade. They have similar nominal yield levels, but the impurity limits, impact test requirements and inspection documents differ, so substitution should always be confirmed against the project specification and the mill certificate.
Can S275JR SHS tube be welded without preheat?
In most thin-wall sections yes, because the carbon equivalent is low. For wall thicknesses above roughly 20 mm, in low ambient temperatures, or when the joint is highly restrained, preheat of 50 - 100 deg C is recommended to avoid hydrogen cracking. Follow the welding procedure qualification for the project.
What is the difference between SHS and RHS tube?
SHS is a square hollow section with equal side lengths; RHS is a rectangular hollow section with unequal sides. Both are covered by EN 10210-1 (hot finished) and EN 10219-1 (cold formed). The choice depends on the direction of the main bending load: RHS can be oriented to give more stiffness in one axis.
Does S275JR have good corrosion resistance?
S275JR offers the same mild atmospheric corrosion resistance as ordinary carbon steel. It will rust outdoors unless protected by paint, galvanizing or other coatings. The copper addition improves resistance to atmospheric corrosion slightly, but S275JR must not be treated as a weathering steel.
What impact test does the JR suffix require?
The JR suffix requires a minimum Charpy V-notch impact energy of 27 J at 20 deg C. If the structure is exposed to lower temperatures, select S275J0 (0 deg C), S275J2 (-20 deg C) or a higher grade as required by the design standard.