The ASTM A312 TP304 Pipe is used for high pressure and high temperature applications because of the high operating temperature of 870 degrees Celsius and the strength.
ASTM A312 is a standard for welded austenitic stainless steel seamless steel pipes. When austenitic stainless steel contains about 18% Cr, 8%~25% Ni, and about 0.1% C, it has a stable austenite structure. Austenitic chromium-nickel stainless steel includes the famous 18Cr-8Ni steel and the high Cr-Ni series steel developed by increasing the Cr and Ni content and adding Mo, Cu, Si, Nb, Ti and other elements. Austenitic stainless steel is non-magnetic and has high toughness and plasticity, but its strength is low. It cannot be strengthened through phase transformation. It can only be strengthened through cold working. If elements such as S, Ca, Se, Te, etc. are added, it has good Easy to cut.
SS DIN 1.4301 Hexagonal Pipe Physical Composition
| Grade | Density (kg/m3) | Elastic Modulus (GPa) | Mean Coefficient of Thermal Expansion (m/m/0C) | Thermal Conductivity (W/m.K) | Specific Heat 0-1000C (J/kg.K) | Electrical Resistivity (n.m) | |||
| 0-1000C | 0-3150C | 0-5380C | at 1000C | at 5000C | |||||
| 304 | 8000 | 193 | 17.2 | 17.8 | 18.4 | 16.2 | 21.5 | 500 | 720 |
Surface Finish of SS 304 Seamless Pipe
| Surface Finish | Internal Surface(ID) | Exterbal Surface(OD) | |||
| Roughness Average(RA) | Roughness Average(RA) | ||||
| μ inch | μm | μ inch | μm | ||
| AP | Annealed & Pickled | Not defined | Not defined | 40 or Not defined | 1.0 or Not defined |
| BA | Beight Annealed | 40,32,25,20 | 1.0,0.8,0.6,0.5 | 32 | 0.8 |
| MP | Mechanical Polish | 40,32,25,20 | 1.0,0.8,0.6,0.5 | 32 | 0.8 |
| EP | Electro Polish | 15,10,7,5 | 0.38,0.25,0.20;0.13 | 32 |
0.8 |