ASTM A333 Low Temperature Grade 6 Steel Pipe

Nov 28, 2025 Leave a message

ASTM A333 Low Temperature Grade 6 Steel Pipe description

A333Gr.6 low-temperature seamless pipe belongs to the category of low-temperature seamless steel pipes. The main application areas of this steel are washing, purification, desulfurization and degreasing production equipment in the production of ethylene, propylene, urea, synthetic ammonia, nitrogen, phosphorus and potassium compound fertilizers and pharmaceutical industries using petroleum, chemical, natural gas and coal as raw materials, as well as cryogenic equipment manufacturing, ultra-low temperature cold storage, pipelines for transporting ultra-low temperature liquefied gases and their pipe components.

 

 

ASTM A333 Gr. 6 Seamless Tube specification

ASTM A333 Gr. 6 chemical composition:

Grades

C.max

Si min

Mn

P

S

Gr. 6

0.30

0.1

0.29-1.06

≤0.025

≤0.025

 

ASTM A333 Gr. 6 mechanical property:

Grades

Tensile strength Rm

Yield strength YS

Enlongation A(%)

Gr. 6

415

240

≥16.5

 

 

The Charpy V-notch (CVN) impact test for A333 GR.6 steel pipe is a core component in verifying its low-temperature toughness. The following is a detailed analysis of the test:

1. Test Standards and Requirements

Standards: ASTM A333/ASME SA333 (clearly specifies the performance requirements for low-temperature steel).

Test Temperature: -50°F (-45°C) (Standard requirement; lower temperatures may be agreed upon separately for specific projects).

Test Direction: Sampling is typically performed along the longitudinal direction (L direction) of the steel pipe to reflect the actual stress state of the pipeline.

2. Specimen Preparation

Sampling Location: Sampling is taken from the pipe body or near the weld (if assessing weld influence). The specific location is determined by the standard or contract.

Specimen Size: The standard Charpy V-notch specimen size is 10mm × 10mm × 55mm (10mm square cross-section, 55mm length), with a V-shaped notch (45° angle, 0.25mm root radius).

Notch Direction: The notch axis is perpendicular to the steel pipe surface, simulating the impact direction the pipe may experience.

3. Test Procedure

Temperature Control: Cool the specimen to -50°F (-45°C) and hold for a sufficient time (usually ≥30 minutes) to ensure the entire specimen reaches the target temperature.

Impact Energy: Use a pendulum impact testing machine to impact the specimen at a specific speed (e.g., 5m/s), and record the energy absorbed when the specimen fractures (unit: J or ft·lbf).

Number of Tests: Typically, 3 specimens are tested per batch of steel pipes, and the average value is taken.

4. Acceptance Criteria

Minimum Absorbed Energy:

Single Specimen: ≥20 ft·lbf (27 J) is a common requirement, but specific values ​​should be referenced from procurement specifications or project standards (some demanding scenarios may require higher values).

Average Value: The average value of 3 specimens must meet or exceed the specified value.

Shear Rate: Some standards require the proportion of shear surface area after specimen fracture (e.g., ≥85%) to determine whether the fracture mode is ductile fracture.

5. Significance of the Test

Verification of Low-Temperature Toughness: Ensures that the steel pipe still has sufficient resistance to brittle fracture at -50°F (-45°C), avoiding sudden failure in low-temperature environments.

Quality Control: Through batch testing, steel pipes that meet the requirements for low-temperature service are selected to ensure project safety.

Design Basis: Test data provides key parameters for the low-temperature design, material selection, and safety assessment of the pipeline system.

test

 